MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NOVA Chemicals Surpass® HPs167-AB Homopolymer sHDPE Film Resin
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes: HPs167-AB complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.

NOVA Chemicals' polyethylene resins are biologically and chemically inert.

Features: Superior barrier properties, Very high stiffness, Low gel

Additives: Antioxidant

Applications: Moisture barrier films, Co-extrusion, Dry food packaging

Film properties are typical of blown film extruded on a 2.5" extruder with 4" die and 35-mil die gap at a blow up ratio of 2:1, but are dependent upon operating conditions.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.966 g/ccASTM D 792
Moisture Vapor Transmission 0.00418 cc-mm/m²-24hr-atm
@Temperature 38.0 °C
100% RH; ASTM F 1249
Oxygen Transmission 1.767 cc-mm/m²-24hr-atm0% RH; ASTM D 3985
Thickness 38.0 micronsAs tested for properties on this data sheet
 25.0 - 75.0 micronsRecommended range for processing
Melt Flow 1.2 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D 1238
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 27.0 MPaASTM D 882
Film Tensile Strength at Yield, TD 25.0 MPaASTM D 882
Elmendorf Tear Strength MD 22 gASTM D 1922
Elmendorf Tear Strength TD 225 gASTM D 1922
Elmendorf Tear Strength, MD 0.580 g/micronASTM D 1922
Elmendorf Tear Strength, TD 5.90 g/micronASTM D 1922
1% Secant Modulus, MD 1100 MPaASTM D 882
1% Secant Modulus, TD 1335 MPaASTM D 882
 
Processing PropertiesOriginal ValueComments
Melt Temperature 200 - 230 °CRecommended
Die Opening 0.0500 - 0.100 inRecommended range
Blow-up Ratio (BUR) 1.5 - 3.0Optimum range
 
Descriptive Properties
Low Friction Puncture19 (J/mm)NOVA Chemicals test method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Petrothene® NA324009 Low Density Polyethylene (Blow Molding Applications)
NOVA Chemicals Surpass® FPs117-C Octene Copolymer sLLDPE Film Resins
NOVA Chemicals Sclair® 99K Homopolymer HDPE Film Resin
NOVA Chemicals Sclair® 19H Homopolymer HDPE Film Resin
NOVA Chemicals Sclair® 19G Homopolymer HDPE Film Resin

PNOV776 / 108901

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.