MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420HC
Categories: Metal; Ferrous Metal; Stainless Steel; T 400 Series Stainless Steel

Material Notes: Allegheny Ludlum Type 420HC is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainless steels. Oil quenching this alloy from temperatures between 1800°F and 1950°F produces the high strength and/or wear resistance as well as corrosion resistance.

A major use for this grade of heat treatable stainless steels is in cutlery. When blanking cutlery parts from annealed raw material stock, Type 420HC will usually exhibit hardness, yield strength, and tensile strength that are low enough for fine blanking purposes. Type 420HC is a high carbon version of Type 420. When sufficient amounts of carbon are added to straight-chromium stainless steel, the alloy then has the capability to transform its microstructure through proper heat treatment (hardening) into one that will possess optimum strength , hardness, edge retention, and wear resistance.

Information provided by Allegheny Ludlum Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.73 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 88
Hardness, Rockwell C 56 - 59
Tensile Strength, Ultimate 600 MPaTypical
Tensile Strength, Yield 310 MPa
@Strain 0.2 %
Elongation at Break 28 %
Modulus of Elasticity 200 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000560 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.2 µm/m-°C
@Temperature 20.0 - 200 °C
 12.5 µm/m-°C
@Temperature 20.0 - 600 °C
Thermal Conductivity 24.207 W/m-K
@Temperature 100 °C
Melting Point 1454 - 1510 °C
Solidus 1454 °C
Liquidus 1510 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.44 %
Chromium, Cr 13 %
Iron, Fe 86 %as balance
Manganese, Mn <= 1.0 %
Nickel, Ni <= 0.50 %
Phosphorus, P <= 0.040 %
Silicon, Si <= 1.0 %
Sulfur, S <= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI E 52100 Steel (100Cr6, SUJ2, UNS G52986)
AK Steel 420HC Martensitic Stainless steel
AISI 4320H Steel, double quenched and tempered: (carburized 925°C (1700°F) for 8 hrs., pot cooled, reheated to 815°C (1500°F), quenched in agitated oil, reheated to 775°C (1425°F), quenched in agitated oil, 230°C (450°F) temper); 1.9 mm case depth
AISI 8620H Steel, quenched from carburizing box, 50 mm (2 in.) round
AISI E9310H Steel, double quenched and tempered at 230°C (450°F), 1.4 mm case depth

NL420H / 17924

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.