MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Park Aerospace Nelcote® F-529 Phenolic Prepreg, 3K PW Reinforced
Categories: Polymer; Thermoset; Phenolic

Material Notes: Nelcote® F-529 is a non-halogenated phenolic resin designed specifically for use in aircraft and mass-transit interior laminate and sandwich panels. F-529 was formulated for applications requiring non-halogenated FST (flame, smoke, toxicity) performance.

Key Features and Benefits:

  • Self-Adhesive resin system for sandwich panel applications
  • Non-Halogenated and antimony-free resin formulation
  • Excellent FST performance
  • Low OSU heat-release (< 20/20)
  • Good Tack and Drape properties
  • White color after cure for superior cosmetics

Applications/Qualifications:

  • Aircraft Interiors
  • Mass-Transit Interiors
  • Meets all requirements of:
    • FAR 25.853
    • FAR 25.856
    • ATS 1000.001
    • OSU 1990

Information provided by Park Electrochemical Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles <= 3.5 %
@Temperature 135 °C
8 min
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 77000 psi
@Temperature 23.9 °C
0° Direction, Dry; Press Cure, 16min, 300°F; ASTM D638
Tensile Modulus 8300 ksi
@Temperature 23.9 °C
0° Direction, Dry; Press Cure, 16min, 300°F; ASTM D638
Compressive Strength 101 ksi
@Temperature 23.9 °C
Dry; Press Cure, 16min, 300°F; ASTM D695
Compressive Modulus 7900 ksi
@Temperature 23.9 °C
Dry; Press Cure, 16min, 300°F; ASTM D695
 
Optical PropertiesOriginal ValueComments
Optical Density 1.0Dm, Flaming Mode; FAR 25.853, Part 25 Appendix F, Part V
 
Processing PropertiesOriginal ValueComments
Gel Time 7.00 min
Shelf Life 6.00 Month
@Temperature 4.44 °C
 
Descriptive Properties
Burn Length (in)1.8Vertical Burn, 60 sec; FAR 25.853, Part 25 Appendix F, Part I (b) (4)
Climbing Drum Peel (in-lb/3in)8ASTM D1781; Dry, 75°F; Press Cure, 16min, 300°F
DripNoneVertical Burn, 60 sec; FAR 25.853, Part 25 Appendix F, Part I (b) (4)
Fabric Area Weight (g/m²)193
Heat Release, Peak (KW/m²)32FAR 25.853 Part 25 Appendix F, Part IV
Heat Release, Total (KW-min/m²)19FAR 25.853 Part 25 Appendix F, Part IV
Prepreg Resin Content (%)38-44
Resin Flow (%)10-30260°F, 150psi
Self Extinguish Time (sec)0Vertical Burn, 60 sec; FAR 25.853, Part 25 Appendix F, Part I (b) (4)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPARK050 / 89322

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.