Description: Preformance® PET 1708HS(A) is a food grade PET copolymer that is suitable for a wide variety of beverage and juice containers hot fill application, high temperature filling. Offers exceptional clarity and color and is engineered for heat-set. The low acetaldehyde content in the resin helps eliminate any impact on aroma and flavor. Preformance® PET 1708HS(A) resin is considered safe for food packaging applications based upon compliance with FDA Regulation 21 CFR Section 177.1630 specifications. |
Exceptional clarity and color |