MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Solvay SIPOMER® B-CEA Beta-Carboxyethyl Acrylate
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: Specialty monomer for Tg modification

Chemical Name: Beta-Carboxyethyl Acrylate

CAS: 24615-84-7

Available in: Asia Pacific, Europe, Latin America and North America

Applications: SIPOMER B-CEA is recommended for use as a functional monomer to provide carboxylic acid groups in copolymers. This monomer is useful for importing latex stability and emulsion copolymer adhesion. It is particularly effective when used as a replacement for other carboxylic acid monomers. While these monomers tend to harden copolymers, Sipomer ß-CEA does not.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 6.1 - 6.7[meq/g]; RP-0008
 
Processing PropertiesOriginal ValueComments
Shelf Life 18.0 Month
 
Component Elements PropertiesOriginal ValueComments
H2O, Water <= 1.0 %Karl fisher; RP-0327
 
Descriptive Properties
AppearanceClear
Color<200APHA, RP-0134
CompositionActive Monomer0.98
 Ester6.4-7.0 meq/g, RP-0496
 MEHQ900-1100 ppm, RP-0301
Foreign MatterFree of foreign matter

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay SIPOMER® WAM II Composition Based On Methacrylamidoethyl Ethylene Urea
Solvay SIPOMER® WAM Allyl / Ureido Monomer
Solvay SIPOMER® SEM 25 Polyalkoxyl Polyarylphenol Ethylenic Methacrylate
Solvay SIPOMER® PAM-4000 Ethylmethacrylate Phosphate; Alkyl Methacrylate Phosphate
Solvay SIPOMER® PAM-300 Phosphate Esters of Ppg Monoacrylate

WRHOD501 / 137732

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.