MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
3M Castable Ceramics
Categories: Ceramic

Material Notes: 3M™ Castable Ceramics are chemically bonded phosphate ceramic products manufactured by Ceradyne, Inc., a 3M company, for use as a neutron poison, shielding material, encapsulant and in waste immobilization applications. These products quickly harden to a tough, high-strength ceramic upon casting and are provided either as a powder blend that can be mixed and cast at the point of use, or as pre-cast form. 3M castable ceramics can be customized with various formulations and additives to provide application-specific characteristics.

Information provided by 3M™

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.91 - 2.00 g/cc
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 3000 - 7000 psi
 
Processing PropertiesOriginal ValueComments
Moisture Content 25 - 27 %
 
Descriptive Properties
AppearanceGray to white ceramic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Less Common Metals Gadolinium Vacuum Remelted Rare Earth Metal
Less Common Metals Gadolinium Sublimed Rare Earth Metal
3M 10B Enriched Boron Oxide

PMM40048 / 194939

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.