MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Nouryon Duomeen T Di-amine, tallow
Categories: Other Engineering Material

Material Notes: Duomeen T is an alkyl diamine.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.806 g/cc
@Temperature 80.0 °C
 0.813 g/cc
@Temperature 70.0 °C
 0.821 g/cc
@Temperature 60.0 °C
Viscosity 7.0 cP
@Temperature 70.0 °C
 8.0 cP
@Temperature 60.0 °C
 10 cP
@Temperature 50.0 °C
Vapor Pressure 0.000013332 bar
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.606 BTU/lb-°F
@Temperature 37.8 °C
 0.617 BTU/lb-°F
@Temperature 60.0 °C
 0.641 BTU/lb-°F
@Temperature 82.2 °C
 0.657 BTU/lb-°F
@Temperature 93.3 °C
Melting Point 44.0 °C
Boiling Point >= 300 °C
@Pressure 0.101325 MPa
Flash Point >= 150 °C
 
Optical PropertiesOriginal ValueComments
Gardner Color Number 0.00 - 7.0
 
Component Elements PropertiesOriginal ValueComments
H2O, Water <= 1.0 %
 
Descriptive Properties
Amine number= 334 mg KOH/g
AppearanceSolid
Content= 45 %Primary Amine
 = 45 %Secondary Amine
 32-50 g I2/100 gIodine value
Equivalent mass0-168
HLB15.6Davies Scale 0-40

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNOURY497 / 286020

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.