MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Teknor Apex Sinelec CCB1002 Low Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Availability: Asia Pacific

Features: Conductive

Uses: Film; Foam

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Film Extrusion; Foam Processing

Preliminary data. Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.00 g/ccASTM D792
Melt Flow 0.50 - 1.8 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ASTM D1238
 4.0 - 9.0 g/10 min
@Load 10.0 kg,
Temperature 190 °C
ASTM D1238
 25 - 42 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 2030 psiASTM D638
Elongation at Break 200 %ASTM D638
Izod Impact, Notched 3.50 ft-lb/inASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 1e+05ASTM D257
Surface Resistance <= 1e+05ASTM D257
 
Processing PropertiesOriginal ValueComments
Zone 1 248 °F
Zone 2 284 °F
Zone 3 302 °F
Zone 4 302 °F
Zone 5 302 °F
Drying Temperature 176 °F
Dry Time 2.00 - 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aclo Accucomp Polyethylene LD0109L Low Density
Multibase Multi-Flam™ 0801 LDPE Polyethylene
Sibur Phenoplast
LATI LATISTAT 43/7-02 Low Density Polyethylene (LDPE) Base Conductive Plastic
Canuck Compounders BK 1-0-3RMF20 Recycled Black Mineral Filled LDPE

PTEKNQ1234 / 237725

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.