MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
SABIC SABIC® PP 37T1030 PP (Global)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: SABIC® PPcompound 37T1030 is a high flow copolymer with 30% talc, offering an excellent balance between stiffness and impact resistance. It has been specially developed for automotive interior parts such as column cladding and door panels. SABIC® PPcompound 37T1030 is a designated automotive grade. IMDS ID: 440839684

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.15 g/ccInjection molded sample ISO527-1A; ISO 1183
Filler Content 30 %SABIC method
Linear Mold Shrinkage 0.0085 cm/cmInjection molded plaque 65x65x3.2mm; SABIC method
Melt Flow 13 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 18.0 MPaISO 527/1A
Tensile Strength, Yield 23.0 MPaISO 527/1A
Elongation at Break 15 %ISO 527/1A
Tensile Modulus 2650 MPaISO 527/1A
Flexural Modulus 2800 MPaISO 178/1A
Izod Impact, Notched (ISO) 4.50 kJ/m²N.B.: No Break; ISO 180/1A
 2.50 kJ/m²
@Temperature -20.0 °C
N.B.: No Break; ISO 180/1A
 3.00 kJ/m²
@Temperature 0.000 °C
N.B.: No Break; ISO 180/1A
Charpy Impact Unnotched 15.0 kJ/m²ISO 179/1eU
Charpy Impact, Notched 5.00 kJ/m²ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear 70.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM D696
 85.0 µm/m-°C
@Temperature -30.0 - 100 °C
ISO 11359-2
 100 µm/m-°C
@Temperature 23.0 - 80.0 °C
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 115 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 130 °CISO 75
Vicat Softening Point 145 °Cat 10 N (VST/A); ISO 306/A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI11448 / 244915

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.