MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
BLUESTAR 101G20 PBT, 20% Glass Filled
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled

Material Notes: Typical Applications: Appliances, molded parts

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.46 g/ccASTM D792
Moisture Absorption at Equilibrium 0.12 %50% RH; ASTM D570
Linear Mold Shrinkage, Flow 0.0040 cm/cmASTM D955
Linear Mold Shrinkage, Transverse 0.013 cm/cmASTM D955
Melt Flow 18 g/10 min
@Load 2.16 kg,
Temperature 250 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 95.0 MPaASTM D638
Tensile Modulus 7100 MPaASTM D638
Flexural Strength 165 MPaASTM D790
Flexural Modulus 6850 MPaASTM D790
Izod Impact, Notched (ISO) 7.00 kJ/m²ASTM D256
Izod Impact, Unnotched (ISO) 43.0 kJ/m²ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 215 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 195 °CASTM D648
Flammability, UL94 HB
@Thickness 0.380 mm
 HB
@Thickness 0.800 mm
 HB
@Thickness 1.60 mm
 HB
@Thickness 3.20 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BLUESTAR 201G20 PBT, 20% Glass Filled
BASF Ultramid® S3EG6 Balance 30% Glass Filled PA 610 (Conditioned)
A. Schulman ComAlloy Hiloy® 431 Glass Reinforced, PBT Alloy
BLUESTAR 403HF-G20 PBT, 20% Glass Filled
BLUESTAR 403G-MG30 PBT, 30% Glass Filled

PBLUE922 / 135344

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.