MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Envalior Durethan® BM 230 H2.0 901510 Nylon 6 (PA6), 30% Mineral Filled, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Mineral Filled

Material Notes: PA 6, injection molding, 30% mineral, isotropic properties, heat-aging stabilized

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.800 g/ccISO 60
Density 1.36 g/ccISO 1183
Moisture Absorption at Equilibrium 2.2 %50% RH; ISO 62
Water Absorption at Saturation 7.0 %IOS 62
Linear Mold Shrinkage, Flow 0.0108 cm/cm150x105x3; 280 °C / MT 80 °C; 500 bar; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0112 cm/cm150x105x3; 280 °C / MT 80 °C; 500 bar; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Puncture Resistance 1132 N
@Temperature -30.0 °C
ISO 6603-2
 4694 N
@Temperature 23.0 °C
ISO 6603-2
Ball Indentation Hardness 180 MPaISO 2093-1
Tensile Strength at Break 80.0 MPa5 mm/min; ISO 527-1,-2
Elongation at Break 10 %5 mm/min; ISO 527-1,-2
Tensile Modulus 5000 MPa1 mm/min; ISO 527-1,-2
Flexural Strength 140 MPa2 mm/min; ISO 178-A
Flexural Yield Strength 130 MPa
@Strain 3.5 %
2 mm/min; ISO 178-A
Flexural Modulus 4700 MPa2 mm/min; ISO 178-A
Flexural Strain at Break 5.5 %2 mm/min; ISO 178-A
Izod Impact, Notched (ISO) <= 10.0 kJ/m²
@Temperature 23.0 °C
ISO 180-1A
 <= 10.0 kJ/m²
@Temperature -30.0 °C
ISO 180-1A
Izod Impact, Unnotched (ISO) 80.0 kJ/m²
@Temperature -30.0 °C
ISO 180-1U
 122 kJ/m²
@Temperature 23.0 °C
ISO 180-1U
Charpy Impact Unnotched 80.0 kJ/m²
@Temperature -30.0 °C
ISO 179-1eU
 120 kJ/m²
@Temperature 23.0 °C
ISO 179-1eU
Charpy Impact, Notched <= 10.0 kJ/m²
@Temperature 23.0 °C
ISO 179 1eA
 <= 10.0 kJ/m²
@Temperature -30.0 °C
ISO 179 1eA
 <= 10.0 kJ/m²
@Temperature -40.0 °C
ISO 179 1eA
Puncture Energy 4.20 J
@Temperature -30.0 °C
ISO 6603-2
 19.1 J
@Temperature 23.0 °C
ISO 6603-2
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+12 ohm-cmIEC 60093
Surface Resistance 1.00e+16 ohmIEC 60093
Dielectric Constant 3.9
@Frequency 1e+6 Hz
IEC 60250
 4.3
@Frequency 100 Hz
IEC 60250
Dielectric Strength 29.0 kV/mm
@Thickness 1.00 mm
IEC 60243-1
Dissipation Factor 0.0080
@Frequency 100 Hz
IEC 60250
 0.018
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 200 VSolution B; IEC 60112
 525 VSolution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
Melting Point 222 °C10°C/min; ISO 11357-1,-3
Deflection Temperature at 0.46 MPa (66 psi) 185 °CISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °CISO 75-1,-2
Deflection Temperature at 8.0 MPa 50.0 °CISO 75-1,-2
Vicat Softening Point >= 200 °C
@Load 5.10 kg
120°C/h; ISO 306
 200 °C
@Load 5.10 kg
50°C/h; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
 HB
@Thickness 3.20 mm
Oxygen Index 25 %Method A; ISO 4589-2
Glow Wire Flammability Index 650 °C
@Thickness 2.00 mm
IEC 60695-2-12
Shrinkage, MD 0.32 %
@Treatment Temp. 120 °C,
Time 14400 sec
Post-Shrinkage Flow Direction 150x105x3; ISO 294-4
Shrinkage, TD 0.30 %
@Treatment Temp. 120 °C,
Time 14400 sec
150x105x3; ISO 294-4
 
Processing PropertiesOriginal ValueComments
Melt Temperature 280 °Cinjection molding
 270 - 290 °C
Mold Temperature 80.0 °Cinjection molding
 80.0 - 120 °C
Drying Temperature 80.0 °C
Dry Time 2.00 - 6.00 hour
Moisture Content 0.030 - 0.12 %Karl Fischer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Minlon® 73M40 NC010 PA6-MD40
EMS-Grivory Grilon® BM-30 PA6-MD30
Envalior Durethan® BM 230 H2.0 901510 Nylon 6 (PA6), 30% Mineral Filled, Conditioned
Celanese Zytel® 73G45L NC010 PA6-GF45
EMS-Grivory Grilon® BG-50 S PA6-GF50

PLANW9440 / 208273

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.