MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Sarlink® TPE RV-2671DN NAT Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Sarlink RV-2671DN NAT is a high performance thermoplastic elastomer, available in NAT and BLK, used in automotive applications, including exterior. Sarlink 2671DN NAT is a high hardness, high density grade exhibiting excellent UV resistance and chemical resistance.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Chemical Resistant; Filled; Good Adhesion; Good Adhesion; Good Mold Release; Good Moldability; Good Processability; Good Processing Stability; Good Toughness; High Density; High Hardness; High Specific Gravity; Low Flow; Lubricated; Light Stabilized; Sunlight Resistant; Slip; UV Resistant; Weather Resistant

Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Profiles; Racks

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Extrusion; Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.12 g/ccISO 1183
Viscosity 665 cP
@Shear Rate 206 1/s,
Temperature 200 °C
ASTM D3835
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 69
@Time 15.0 sec
Injection Molded; ISO 868
 71
@Time 5.00 sec
Injection Molded; ISO 868
 73
@Time 1.00 sec
Injection Molded; ISO 868
 70.7
@Treatment Temp. 110 °C,
Time 15.0 sec
Change in Air, 1008 hr; ISO 888
 70.7
@Treatment Temp. 125 °C,
Time 15.0 sec
Change in Air, 168 hr; ISO 888
 72.4
@Treatment Temp. 110 °C,
Time 5.00 sec
Change in Air, 1008 hr; ISO 888
 72.6
@Treatment Temp. 125 °C,
Time 5.00 sec
Change in Air, 168 hr; ISO 888
 73.6
@Treatment Temp. 110 °C,
Time 1.00 sec
Change in Air, 1008 hr; ISO 888
 74.3
@Treatment Temp. 125 °C,
Time 1.00 sec
Change in Air, 168 hr; ISO 888
Tensile Strength at Break 2840 psiAcross Flow, Type 1, 20 in/min; ISO 37
 3450 psiFlow, Type 1, 20 in/min; ISO 37
 3000 psi
@Treatment Temp. 125 °C,
Time 605000 sec
Across Flow, Type 1, Change in Air; ISO 188
 3150 psi
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
Across Flow, Type 1, Change in Air; ISO 188
 3420 psi
@Treatment Temp. 125 °C,
Time 605000 sec
Flow, Type 1, Change in Air; ISO 188
 3520 psi
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
Flow, Type 1, Change in Air; ISO 188
Tensile Stress at Strain 2060 psi
@Strain 100 %
Across Flow, Type 1, 20 in/min; ISO 37
 2210 psi
@Strain 100 %
Flow, Type 1, 20 in/min; ISO 37
 2310 psi
@Strain 100 %,
Treatment Temp. 110 °C
Across Flow, Type 1, Change in Air, 1008 hr; ISO 188
 2500 psi
@Strain 100 %,
Treatment Temp. 125 °C
Across Flow, Type 1, Change in Air, 6.61 in; ISO 188
 3230 psi
@Strain 100 %,
Treatment Temp. 110 °C
Flow, Type 1, Change in Air, 1008 hr; ISO 188
 3290 psi
@Strain 100 %,
Treatment Temp. 125 °C
Flow, Type 1, Change in Air, 168 hr; ISO 188
Elongation at Break 90.2 %
 110 %Across Flow, Type 1, 20 in/min; ISO 37
 119 %
 140 %Flow, Type 1, 20 in/min; ISO 37
Flexural Yield Strength 4660 psiISO 178
Flexural Modulus 264000 psiISO 178
Tear Strength 780 pliFlow, Method Ba, Angle (Unnicked), 20 in/min; ISO 34-1
 940 pliAcross Flow, Method Ba, Angle (Unnicked), 20 in/min; ISO 34-1
Compression Set 46 %
@Temperature 22.8 °C,
Time 79200 sec
Type 1; ISO 815
 74 %
@Temperature 125 °C,
Time 252000 sec
Type 1; ISO 815
 77 %
@Temperature 90.0 °C,
Time 252000 sec
Type 1; ISO 815
 78 %
@Temperature 70.0 °C,
Time 79200 sec
Type 1; ISO 815
 
Processing PropertiesOriginal ValueComments
Processing Temperature 380 - 450 °FInjection, Melt
Rear Barrel Temperature 380 - 450 °FInjection
Middle Barrel Temperature 380 - 450 °FInjection
Front Barrel Temperature 380 - 450 °FInjection
Nozzle Temperature 380 - 450 °FInjection
Zone 1 380 - 430 °FExtrusion
Zone 2 380 - 430 °FExtrusion
Zone 3 380 - 430 °FExtrusion
Zone 4 380 - 430 °FExtrusion
Zone 5 380 - 430 °FExtrusion
Die Temperature 380 - 430 °FExtrusion
Mold Temperature 60.0 - 110 °FInjection
Injection Pressure 200 - 1000 psiInjection
Back Pressure 25.0 - 50.0 psiInjection
Cushion 0.150 - 1.00 inInjection
Screw Speed 50 - 100 rpmInjection
 
Descriptive Properties
AppearanceBlack
 Natural Color
 Opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ1129 / 237620

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.