MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
3M Weatherban™ 5354 Sealant Tape
Categories: Polymer; Adhesive

Material Notes:
  • 3M™ Weatherban™ Sealant Tape 5354 is a high tack extruded synthetic rubber, non-curing sealant in tape form.
  • It can be used to seal between glass, metal, wood and many plastics.
  • Easy to compress and has exceptional cold flow resistance.
  • Good adhesion to dry surfaces and will stay in place when positioned vertically, overhead or around sharp corners.
  • Low moisture vapor transmission.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.41 g/cc
Solids Content 100 %
Water Vapor Transmission 0.390 g/m²/dayASTM E96-66
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore OO 60
 62
@Treatment Temp. 110 °C,
Time 605000 sec
Heat Aging
Shear Strength 7.00 psi
@Temperature 110 °C,
Time 605000 sec
Overlap
 10.4 psi
@Temperature 110 °C,
Time 605000 sec
Overlap
 10.9 psi
@Temperature 110 °C,
Time 605000 sec
Overlap
 11.9 psi
@Temperature 110 °C,
Time 605000 sec
Overlap
 13.0 psi
@Temperature 110 °C,
Time 605000 sec
Overlap
 7.00 psi
@Time 86400 sec
Overlap
 10.0 psi
@Time 86400 sec
Overlap
 10.0 psi
@Time 86400 sec
Overlap
 10.5 psi
@Time 86400 sec
Overlap
 10.5 psi
@Time 86400 sec
Overlap
 
Processing PropertiesOriginal ValueComments
Shelf Life 15.0 Month
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMM33170 / 167917

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.