MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Gougeon Brothers West System® 105 Epoxy Resin® / 209 Extra Slow Hardener®
Categories: Polymer; Thermoset; Epoxy

Material Notes: 105/209 Epoxy is used for general coating and bonding applications in extremely warm and/or humid conditions or when extended working time is desired at room temperature. Provides approximately twice the working time of 206 Slow Hardener. 105/209 forms a high-strength, moisture-resistant solid with excellent bonding and barrier coating properties. It will wet out and bond to wood fiber, fiberglass, reinforcing fabrics, foam and other composite materials, and a variety of metals. 105/209 Epoxy can be thickened with WEST SYSTEM fillers to bridge gaps and fill voids and can be sanded and shaped when cured. With roller applications, it has excellent thin-film characteristics, allowing it to flow out and self-level without “fish-eyeing.” Multiple coats of 105/209 Epoxy creates a superior moisture barrier and a tough, stable base for paints and varnishes. It is formulated without volatile solvents resulting in a very low VOC content. It has a relatively high flash point, no strong solvent odor and does not shrink after curing. It is not intended for clear coating natural finished wood.

Information provided by Gougeon Brothers, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.16 g/cc
Solids Content 93.9 - 99.9 %Volume
Volatile Organic Compounds (VOC) Content 19.3 g/lEPA Method 24; ASTM 2369-93
Viscosity 650 cPMixed; ASTM D-2393
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 82ASTM D-2240
Tensile Strength 7300 psiASTM D638
Elongation at Break 3.6 %ASTM D638
Tensile Modulus 398000 psiASTM D638
Flexural Strength 12500 psiASTM D-790
Flexural Modulus 397000 psiASTM D-790
Compressive Yield Strength 12000 psiASTM D-695
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 21.0 °C
Deflection Temperature at 0.46 MPa (66 psi) 117 °FASTM D-648
Glass Transition Temp, Tg 122 °FOnset
 130 °FUltimate
 
Processing PropertiesOriginal ValueComments
Cure Time 20.0 - 24.0 hoursolid, thin film
 96.0 - 216 hourworking strength
Pot Life 40.0 - 50.0 min100 g
Working Life 3.00 - 4.00 hourThin film
 
Descriptive Properties
Annular shear fatigue9900 lb@ 100,000 cycles
Mix ratio3 parts resin: 1 part hardenervolume, 300 Mini Pump ratio
 3.68 : 1weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGOUGW905 / 290749

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.