Description: Formadur® PH X Superclean is a corrosion-resistant, martensitic precipitation hardened stainless steel Characteristics: Excellent resistance to corrosion; Excellent polishability; Excellent dimensional stability; Good strength; and Good toughness Applications: Formadur® PH X Superclean is recommended for tools/molds for the processing of corrosive plastics. Information provided by Schmolz + Bickenbach |