(Viewing data as-entered.
Click here
to return)
Kazanorgsintez E-9 Petroleum Resin
Categories:
Other Engineering Material
;
Additive/Filler for Polymer
Material Notes:
Production Method:
Obtained as a by-product in the process of hydrocarbon gas pyrolysis on ethylene production plants.
Application:
Feedstock for production of motor fuel, solvents and aromatic hydrocarbons.
Information Provided by Kazanorgsintez
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
>=
0.800
g/cc
@Temperature 20.0 °C
Thermal Properties
Original Value
Comments
Boiling Point
>=
35.0
°C
Initial
<=
220
°C
End
Component Elements Properties
Original Value
Comments
Free Water
<= 1.0 %
Descriptive Properties
Appearance
Liquid of light-yellow to brown color, free of mechanical impurities
Mass Content (%)
40
Mass content of benzene
55
Mass content of aromatic hydrocarbons (C6-C8)
Volume ratio of fraction, in strippant up to 185°C (%)
35
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PKAZAN106 / 127425
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.