MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
HB Fuller HL2278 Hot Melt Adhesive
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: HL2278 is a solvent-free, UL recognized spray grade hot melt adhesive for bonding insulation to painted and unpainted metal. It contains no fillers and provides improved spray characteristics over filled adhesives.

Features and Benefits:

  • UL recognized.
  • Excellent performance for spray application
  • Good bond strength on a variety of substrates
  • Excellent for bonding insulation to painted and unpainted metal and galvanized metal
  • Low/no residue after removal
  • Excellent removability

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 100 %
Viscosity 13750 cP
@Temperature 177 °C
 33500 cP
@Temperature 163 °C
 117500 cP
@Temperature 149 °C
 
Mechanical PropertiesOriginal ValueComments
Peel Strength 7.00 pli180 Degree Peel (60s/75ºF, 0.001 in)
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 350 °F
Flash Point 235 °CCleveland Open Cup
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
ColorLight Amber
ConsistencyViscous LiquidSolid at Room Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHBFULL170 / 316961

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.