MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
ITW Spraycore® SC PDR 6000 Polyester Adhesive
Categories: Polymer; Thermoset; Polyester, TS

Material Notes: SC PDR 6000 Adhesive Putty is a strong ultra light polyester adhesive putty that is primarily used to bond fiberglass parts. MEKP catalyst is not included. Product features: formulated to gel and cure evenly in both thick and thin cross sections, smooth creamy texture allows for easy spreading without tearing, offers low shrinkage and low exothermic, has great bonding characteristics. Product benefits: has great vertical hang without sagging in thick applications, can be cast very thick cross sections without cracking. Preferred red dye catalyst: DDM-9, MEKP-9, DDM-30.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 6.10 - 6.60 lb/galApplication density
Viscosity 600000 - 700000 cPRVT T-E@5rpm
 
Chemical PropertiesOriginal ValueComments
Styrene Content 25 %
 
Processing PropertiesOriginal ValueComments
Gel Time 15.0 - 30.0 minGel to Peak
 75.0 - 105 min
 
Descriptive Properties
Colorwhite
Peak Exotherm200 to 250°F100g mass

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PITWS9051 / 239561

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.