MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
CMT Materials HYTAC® Rx-H1 High Stick Pharmaceutical Grade Syntactic Plug Material  (discontinued **)
Categories: Polymer

Material Notes: HYTAC-Rx is a new syntactic plug assist material developed solely for pharmaceutical blister packaging. HYTAC-Rx syntactics are food contact grade materials and are listed in CMT Materials, Inc. Drug Master File (DMF) number 21370. Plug assist tooling manufactured with HYTAC-Rx material aids in the thermoforming process, resulting in more uniform material distribution and improved barrier performance.

Developed to meet the specific demands of the pharmaceutical packaging industry, HYTAC-Rx is available in both a high-slip and a high-stick formulation. These material options provide the manufacturer with greater control over the thermoforming process, and the ability to optimize plug assist tooling for better material distribution and performance. This improvement may also result in the ability to down-gage film thickness providing substantial cost savings, especially with some of the new, higher priced multi-layer films.

The high stick formulation, HYTAC-Rx-H1, allows the plug to move more material into the formed product when single or multi-layer sheet material requires it. HYTAC-Rx-H1 is also designed for improved toughness and ease of machining. The high slip formulation, HYTAC-Rx-L1 provides more slip as well as improved release properties for sheets that exhibit heavy bottoms or plug sticking problems. HYTAC-Rx-L1 is also designed for higher compressive strength, lower CTE and higher temperature resistance for highly detailed plugs.

Syntactic materials have long been used to fabricate plug assists in the thin gage thermoforming industry to produce cups, containers, and packaging for the food, medical, electronic and consumer markets. HYTAC-Rx is the first and only material designed for pharmaceutical blister tooling.

Information Provided by CMT Materials, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 47.0 - 51.0 lb/ft³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 85
Compressive Strength 14050 psi
Compressive Modulus 380 ksi
 
Thermal PropertiesOriginal ValueComments
CTE, linear 25.3 µin/in-°F
Specific Heat Capacity 0.280 BTU/lb-°F
Thermal Conductivity 0.140 W/m-K
Maximum Service Temperature, Air 350 °F
 
Descriptive Properties
ColorCream

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCMTZ005 / 93145

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.