MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Saint-Gobain Chemfab® SlipGrip™ 10 PTFE/Silicone Coated Fiberglass Fabric
Categories: Ceramic; Glass; Glass Fiber

Material Notes: Description: SlipGrip™ products are PTFE-coated fiberglass fabrics with silicone rubber on one face. This unique combination provides a "slippery" PTFE surface and a "grippy" silicone surface. Both surfaces exhibit superior release and inert properties. SlipGrip products have a variety of uses, including release sheets, belting gasketing, diaphragms, and protective matting.

Specification Notes: The data listed is for reference only. It is not a guarantee of product performance. All data based on a 0.012 inch test sample.
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 48.61 - 62.5 lb/ft³
 
Mechanical PropertiesOriginal ValueComments
Tear Strength Test 8.0Lbs./In. for warp/longitudinal Propagation Tear Strength
 8.0Lbs./In. Propagation Tear Strength in fill/transverse direction
Tear Strength 175 pliTensile Strength (Fill)
 225 pliTensile Strength (Warp)
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 500 °F
 
Descriptive Properties
Weight (oz/yd^2)17

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Saint-Gobain Chemfab® 1584G PTFE Coated Fiberglass Conveyor Belting
Saint-Gobain Chemfab® 1565V PTFE Coated Fiberglass Conveyor Belting
Saint-Gobain Chemfab® 1584N PTFE Coated Fiberglass Conveyor Belting
Saint-Gobain Chemfab® 1589 PTFE Coated Fiberglass Conveyor Belting
NeoGraf GRAFOIL® UCAR®-323 Reinforced PTFE Gasketing

CSTGQZ121 / 2250

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.