MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Teknor Apex Sinpolene FRF2074 Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Flame Retardant

Material Notes: Availability: Africa & Middle East; Latin America; Asia Pacific; South America

Features: Flame Retardant

Uses: Appliance Components; Housings

Forms: Pellets

Information Provided by Teknor Apex

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.938 g/ccASTM D792
Linear Mold Shrinkage 0.00013 in/inASTM D955
Melt Flow 9.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 87ASTM D785
Tensile Strength, Yield 5510 psiASTM D638
Flexural Strength 5800 psiASTM D790
Flexural Modulus 189000 psiASTM D790
Izod Impact, Notched 0.470 ft-lb/in
@Temperature 22.8 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 221 °FUnannealed; ASTM D648
Vicat Softening Point 309 °FLoading 1 (10N); ASTM D1525
Flammability, UL94 V-2
@Thickness 1.60 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Tisan TISOPLEN® Flame Retardant (V0). Heat Stabilized, Copolymer Polypropylene
Tipco Tipcolene® PP FR V0 - UL94-V0 Flame Retardant Polypropylene Homopolymer
Techmer ES HiFill FR® PP FR-N X BKN001
SPS Guang Zhou SAMAT™ 5003 Flame-retarded Polypropylene
Overview of materials for Polypropylene, Flame Retardant

PTEKNP227 / 129308

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.