MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Chi Mei Kibisan® PN-117 SAN  (discontinued **)
Categories: Polymer; Thermoplastic; SAN Polymer; Styrene Acrylonitrile (SAN), Molded

Material Notes: Injection Molding

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.06 g/ccISO 1183
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cmASTM D955
Melt Flow 2.8 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 14 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ASTM D1238
 32 g/10 min
@Load 10.0 kg,
Temperature 220 °C
Melt Volume Rate (ml/10 min); ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 83ASTM D790
Ball Indentation Hardness 159 MPaH358/30; ISO 2039-1
Tensile Strength at Break 64.0 MPa50 mm/min; ISO 527
Tensile Strength, Yield 68.0 MPa50 mm/min; ISO 527
 10060 psi
@Thickness 3.17 mm
ASTM D638
Elongation at Break 6.0 %50 mm/min; ISO 527
Flexural Strength 93.0 MPa2 mm/min; ISO 178
Flexural Yield Strength 14200 psi
@Thickness 3.17 mm
ASTM D790
Flexural Modulus 2.70 GPa2 mm/min; ISO 178
Izod Impact, Notched 0.310 ft-lb/in
@Thickness 6.35 mm,
Temperature 23.0 °C
ASTM D256
 0.330 ft-lb/in
@Thickness 3.17 mm,
Temperature 23.0 °C
ASTM D256
Izod Impact, Notched (ISO) 3.00 kJ/m²ISO 180/1A
Izod Impact, Unnotched (ISO) 15.0 kJ/m²ISO 180/1C
Charpy Impact Unnotched 2.00 J/cm²ISO 179
Charpy Impact, Notched 0.200 J/cm²ISO 179
Impact 3.0Impact Flexural Test Notched (KJ/m²)
 19Impact Flexural Test Unnotched (KJ/m²)
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 86.0 °Cunannealed; ISO 75
 97.0 °Cannealed; ISO 75
Vicat Softening Point 102 °C
@Load 5.00 kg
50°C/hr; ISO 306
 104 °C
@Load 5.00 kg
120°C/hr; ISO 306
 106 °C
@Load 1.00 kg
50°C/hr; ISO 306
 109 °C
@Load 1.00 kg
120°C/hr; ISO 306
Flammability, UL94 HB
@Thickness 1.59 mm
 HB
@Thickness 1.59 mm
UL 94

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chi Mei Kibisan® PN-127 SAN
Chi Mei Kibisan® PN-107 L125 SAN
INEOS Styrolution Luran® HH-120 Alpha-Methylstyrene Acrylonitrile
Chi Mei Kibisan® PN-106 L150 SAN
Chi Mei Kibisan® PN137H SAN Resin, General Purpose

PCHI975 / 109463

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.