MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Okulen® OKULEN® 2000 – L plus – grey – FN7020 UHMW-PE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes: OKULEN® 2000-L plus is a oil filled UHMW Polymer. This material was designed for the conveying industry. The enhanced lubricated oil filler helps on high speed chains or heavy dry run areas of the conveyor. Further, it helps reduce noise levels with its excellent gliding properties. This UHMW is known for its great impact strength and abrasion resistance surface quality.

Properties: Good abrasion resistance; Great gliding properties; Water repellent; Great noise reduction; Lubricant stays on surface (oil), N

Color: grey FN7010; OK-Nr 7010

Range of applications: Conveyor industry, Bearings

Information provided by Okulen

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.930 g/cc0.0336 lb/in³DIN EN ISO 11831-1
Water Absorption <= 0.010 %<= 0.010 %DIN EN ISO 62
Molecular Weight 9.00e+6 g/mol9.00e+6 g/mol
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 58 - 60
@Time 3.00 sec
58 - 60
@Time 0.000833 hour
6 mm plate; DIN EN ISO 868
Tensile Strength, Yield >= 16.0 MPa>= 2320 psi1B- 50 mm/min; DIN EN ISO 527-2
Elongation at Break >= 200 %>= 200 %1B- 50 mm/min; DIN EN ISO 527-2
Tensile Modulus >= 0.300 GPa>= 43.5 ksi1B- 1 mm/min; DIN EN ISO 527-2
Izod Impact, Notched (ISO) >= 80.0 kJ/m²>= 38.1 ft-lb/in²DIN EN ISO 21304-2
Coefficient of Friction, Dynamic 0.0900.090ASTM D1894
Coefficient of Friction, Static 0.150.15ASTM D1894
Abrasion 8080Sand-Slurry; DIN EN ISO 15527
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cmDIN EN 62631-3-1
Surface Resistance >= 1.00e+13 ohm>= 1.00e+13 ohmDIN EN 62631-3-2
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 15.0 - 20.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
8.33 - 11.1 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359
Thermal Conductivity 0.410 W/m-K2.85 BTU-in/hr-ft²-°F
Melting Point 135 - 137 °C275 - 279 °FDIN EN ISO 11357-1
Flammability, UL94 HBHB
 
Descriptive Properties
Operation Temperature80°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

POKUL1038 / 307315

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.