MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Shinil Chemical SHINCON PEEK-CF LCD Rack
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Carbon Fiber Filled

Material Notes: LCD Rack is used to transfer or bake LCD frame in the electronic assembly or LCD packaging assembly line. Current LCD Rack is made of poly ether ether ketone (PEEK) with carbon fiber (CF). Since both materials cost high, there is a need to design the material with cost effectiveness. Also, the current LCD Rack has a concern of sloughing by CF particulates. SHINIL sloves these problems with the CNT composite of polyphenylene sulfide (PPS), polyether sulfone (PES), PEEK, or polyether imide (PEI) by providing the cost effectiveness combined with enhanced mechanical properties. Especially, the wear resistance (coefficient of friction, coefficient of abrasion) of SHINIL CNT composite was much lower than the current PEEK material, which will provide the material for clean/dust free LCD operation environments.

    Features and Benefits
  • Permanent electro conductivity
  • Improved mechanical properties
  • No particulates and no sloughing
  • Lighter weight
  • Recyclability
  • Low abrasion and friction
  • Improved surface
  • Cost effective

Information Provided by Shinil Chemical Industry Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.43 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 2500 kg(f)/cm²
Flexural Strength 343.35 MPa
Flexural Modulus 180000 kg(f)/cm²
Izod Impact, Notched 9.00 kg-cm/cm
Coefficient of Friction, Dynamic 0.166
@Time 3600 sec,
Pressure 1.96 MPa
0.2 m/s
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1e+05
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 240 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 390 °C
 
Descriptive Properties
Abrasion Weight (g)0.0015Wear Tester 0.2m/s; 20kgf/cm2; 1hr
Coefficient of Abrasion (10-3 cm2-sec/kgf-m-hr)0.1358Wear Tester 0.2m/s; 20kgf/cm2; 1hr

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Jushi E7 DR-380 Direct Roving - Epoxy Composite
DuPont Mobility and Materials Vespel® CP-9800 Carbon Fiber and Epoxy Composite, Ultra-high modulus end effectors
DuPont Mobility and Materials Vespel® CP-0648 Polyimide
DuPont Mobility and Materials Vespel® CP-0644 Polyimide
DuPont Mobility and Materials Zytel® HTN 54G35EF NC010 Polyphthalamide (PPA)

PSHINL04 / 104006

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.