MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Escorene™ LD 730.09 Blown Ethylene Vinyl Acetate Copolymer
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: Product Description: Escorene Ultra LD 730.09 is a 17.2% vinyl acetate copolymer film resin. LD 730.09 is designed to have superior strength and toughness combined with excellent optics and sealing properties.

Availability: Latin America, North America and South America

Additive:

  • Antiblock: No
  • Slip: No
  • Thermal Stabilizer: Yes
Applications:
  • Heat Seal Layer
  • Pallet Shrink Film
  • Stretch Film

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.939 g/ccExxonMobil method
Vinyl Acetate Content 17.2 %ExxonMobil method
Melt Flow 0.70 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 370 %ASTM D882
Film Elongation at Break, TD 660 %ASTM D882
Elmendorf Tear Strength MD 50 gASTM D1922
Elmendorf Tear Strength TD 120 gASTM D1922
Dart Drop Test 650 gASTM D1709A
Film Tensile Strength at Break, MD 5300 psiASTM D882
Film Tensile Strength at Break, TD 5300 psiASTM D882
1% Secant Modulus, MD 9200 psiASTM D882
1% Secant Modulus, TD 10000 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point <= 189 °FPeak Melting Point; ExxonMobil method
Vicat Softening Point 153 °FASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 1.3 %ASTM D1003
Gloss 87 %45°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Eurofoam Evacell EVA 30 EVA + PE Foam
ExxonMobil Escorene® LD 721.IK Film Resin
ExxonMobil Escorene™ 768.MJ Blown Ethylene Vinyl Acetate Copolymer
ExxonMobil Escorene® LD 701.ID Blown Film Resin
Eurofoam Evacell EVA 100 EVA + PE Foam

PEX99068 / 175304

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.