MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
3M Cold Seal® 4130 Polyethylene Tape
Categories: Polymer; Adhesive

Material Notes: 3M™ Cold Seal® Polyethylene Tape 4130 is a temporary tape with a self-sealing latex emulsion and feature a self-adhering cohesive coating which bonds to itself and not to the product to be packaged and the result is an airtight pouch that is resistant to moisture, dirt and grease.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 4.00 milASTM D3652
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 1.70 MPaASTM D3759
Elongation at Break 450 %ASTM D3759
Peel Strength 0.8571 pliAdhesion to Steel; ASTM D3330
 
Descriptive Properties
Adhesive TypeNatural rubber latex emulsion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M 5423 Polyethylene Tape
DuPont Mobility and Materials AquaStik® AQS-2900 Polychloroprene Latex
DuPont Mobility and Materials AquaStik® AQS-2540 Polychloroprene Latex
AISI 4140 Steel, normalized at 870°C (1600°F), reheated to 845°C (1550°F), oil quenched, 650°C (1200°F) temper, 25 mm (1 in.) round
AISI 4130 Steel, normalized at 870°C (1600°F), air cooled, 100 mm (4 in.) round

PMM34387 / 169134

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.