MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Selenis VENUZ EB 700 Copolyester for Cosmetics Packaging
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Selenis Venuz EB 700 copolyester has been specifically developed for injection blow molding process of bottles and containers of any shape for the cosmetics industry, such as mascara bottles, lip gloss and lipstick containers and eyeliner cases. Selenis Venuz EB 700 offers exceptional clarity, neutral color and high gloss, granting enhanced shelf appeal whilst protecting product ingredients. Packages will stand out of the shelf even if colored, thanks to the high glossy finish that is achievable with Selenis Venuz EB 700. Cosmetic parts molded from Selenis Venuz EB 700 provide good chemical resistance to most ingredients used in the industry as well as good barrier properties, helping brand owners grant product safety and preservation during storage. Selenis Venuz EB 700 provides good impact resistance allowing unique and personalized designs. Selenis Venuz EB 700 grade may be easily processed on standard blow molding machines, provided appropriate drying equipment is used.

Information provided by Selenis.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.730 g/cc
Density 1.29 g/ccASTM D792 (2013)
Moisture Absorption at Equilibrium <= 0.30 %
Viscosity Test 78 - 82 cm³/gIntrinsic; ISO 1628-5
ASTM Color <= 1.0b*; ASTM D6290
 >= 64L*; ASTM D6290
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 80.0 °CASTM D3418
 
Processing PropertiesOriginal ValueComments
Melt Temperature 180 - 250 °C
Drying Temperature <= 70.0 °Cto avoid chips sticking together in dryer hopper
 60.0 - 65.0 °C
@Time 21600 - 28800 sec
Moisture Content <= 0.0040 %dried
Dew Point -40.0 °C
 
Descriptive Properties
Food Approval PharmacopeiaYes
Particle size320 ± 50 mg/20 chips
Pellet ShapeCylindrical

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSELE933 / 243431

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.