Styrolux® 3G46 is a clear styrene-butadiene copolymer (SBC) developed specifically for sheet- and film extrusion and for thermoformed articles. Styrolux® 3G46 is designed for improved performance in blends with general-purpose polystyrene, providing parts with an excellent balance of transparency and toughness. Outstanding clarity, Good toughness / stiffness balance, Medium GPPS blend capability. Applications: Food and non-food packaging, Caps and lids, Toys, Displays, Medical devices, Household products.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |