The specialty polypropylene Clyrell product portfolio includes random and impact copolymers based on Ziegler-Natta catalysts. Clyrell RC3254 is a polypropylene random copolymer used for extrusion applications. Clyrell RC3254 is formulated with an anti-gasfading stabilization package and is used for the production of textile filaments with high softness. Typical application is nonwovens. Applications: Filament Yarn, Hygiene Nonwoven, Nonwovens.Information provided by LyondellBasell. |