MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Carmel Olefins CARMELCOAT™ MT 34 EC Specialty Polypropylene for Extrusion Coating
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Extrusion Grade

Material Notes: CARMELCOAT™ MT 34 EC is a specialty polypropylene developed for extrusion coating and lamination. This grade exhibits improved process ability for applications which requires high coating speeds, low coating weight, low neck-in, good adhesion to substrate and high temperature resistance.

APPLICATIONS

CARMELCOAT ™ MT 34 EC is suitable for extrusion coating and lamination of paper, paperboards, plastic film, woven PP cloths, and PP based nonwoven fabrics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.910 g/ccASTM D1505
Melt Flow 25 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Flexural Modulus 1025 MPaASTM D790
Izod Impact, Notched 23.0 J/m
@Temperature >=23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °CASTM D648
Vicat Softening Point 132 °C
@Load 1.02 kg
ASTM D1525
 
Processing PropertiesOriginal ValueComments
Die Temperature 310 °C
Melt Temperature 280 - 330 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
IRPC Polimaxx Polene 3375RM Polypropylene Random Copolymer
PolyMirae Moplen HP310R Extrusion Coating and Lamination Grade Polypropylene
IRPC Polimaxx Polene 3370RM Polypropylene Random Copolymer
Esenttia 25C35-EC Impact Block Copolymer Polypropylene
Reliance Industries Repol B250EG Polypropylene

PCARM036 / 79774

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.