MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Total 6671XBB Polypropylene, Cast Extrusion Grade  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Random copolymer film grade

Color - Low catalyst residuals in FINA 6671XBB result in improved color stability.

Clarity/Impact - The random copolymer structure of FINA 6671XBB improves its clarity and impact resistance over conventional homopolymer films.

Slip/Antiblock - FINA 6671XBB is formulated with medium slip and medium antiblock for improved film handling.

FDA - FINA 6671XBB complies with all applicable FDA regulations for food contact applications.

Recommended Applications - FINA 6671XBB is recommended for use in non-oriented cast film processes for manufacture of packaging films that require improved optical and impact properties.

Processing - FINA 6671XBB resin processes on cast extrusion equipment with typical melt temperatures of 450-525°F (232-274°C)

Data provided by the manufacturer, Total Petrochemicals.

Total Petrochemicals includes former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D1505
Melt Flow 11 g/10 minASTM D1238L
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 450 %Non-oriented film; ASTM D882
Secant Modulus 0.590 GPa3 mil film; ASTM D882
Film Tensile Strength at Break, MD 33.1 MPaOrientation not specified. 3 mil film; ASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 148 °CDSC
 
Optical PropertiesOriginal ValueComments
Haze 1.7 %Non-oriented film; ASTM D1003
Gloss 87 %45°; Non-oriented film; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Melt Temperature 232 - 274 °Ccast extrusion

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Braskem H 401 Cast Film Extrusion Polypropylene
ExxonMobil PP1364E2 Polypropylene Homopolymer
Ineos H07G-00 Polypropylene Homopolymer
INEOS Styrolution PS 165 N/L GPPS
INEOS Styrolution PS 158 N/L GPPS

PFIN82 / 38412

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.