MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chase Electronic Coatings HumiSeal® 2C51 Silicone Conformal Coating
Categories: Polymer; Thermoset; Silicone

Material Notes: HumiSeal® 2C51 is a two component high strength, fast curing silicone encapsulating gel supplied as Parts A and B, suitable for general printed circuit board applications. HumiSeal® 2C51 is characterized by room temperature cure and low viscosity for ease of application and contains UV tracer for ease of inspection. The two components of HumiSeal 2C51 are blue and yellow and turn green when mixed. HumiSeal® 2C51 is RoHS Directive 2011/65/EC compliant.

Information provided by Chase Electronic Coatings.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.970 g/ccASTM D1475
Solids Content 99 %By weight; Fed-Std-141, Meth. 4044
Volatile Organic Compounds (VOC) Content 0.00 g/l
Viscosity 200 - 350 cPFed-Std-141, Meth. 4287. Part A
 400 - 700 cPFed-Std-141, Meth. 4287. Part B
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore OO 45 - 55
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 5.20e+13 ohm-cmASTM D257
 
Processing PropertiesOriginal ValueComments
Cure Time 0.500 hour
@Temperature 70.0 °C
Optimum Properties
Tack-Free Time 0.170 hourFed-Std-141, Meth. 4061
Gel Time 8.00 - 10.0 min
@Temperature 23.0 °C
Shelf Life 12.0 Month
@Temperature 23.0 °C
DOM

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHAS927 / 239788

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.