MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Domo TECHNYL® A 218 V35 Black 21 N PA 66 35% Glass Reinforced, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 40% Glass Fiber Filled; Nylon 66, Heat Stabilized

Material Notes: Description: TECHNYL® A 218 V35 Black 21 N is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in black color.

Key Properties: Mechanical performance; Heat stabilized

Benefits: The product offers an excellent combination between thermal and mechanical properties.

Applications: It is used in a wide variety of industries.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.41 g/ccASTM D792
Water Absorption 0.75 %
@Time 86400 sec
ISO 62
Viscosity 22 cP
@Shear Rate 10000 1/s,
Temperature 300 °C
 23.2 cP
@Shear Rate 10000 1/s,
Temperature 290 °C
 24 cP
@Shear Rate 10000 1/s,
Temperature 280 °C
 200 cP
@Shear Rate 100 1/s,
Temperature 300 °C
 222 cP
@Shear Rate 100 1/s,
Temperature 290 °C
 300 cP
@Shear Rate 100 1/s,
Temperature 280 °C
Linear Mold Shrinkage 0.0060 cm/cmIsotropy
Linear Mold Shrinkage, Flow 0.0045 cm/cm
Linear Mold Shrinkage, Transverse 0.0075 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 210 MPaISO 527 Type 1A
Tensile Stress at Strain 40.0 MPa
@Strain 1.5 %,
Temperature 150 °C
 40.0 MPa
@Strain 1.4 %,
Temperature 120 °C
 70.0 MPa
@Strain 2 %,
Temperature 150 °C
 75.0 MPa
@Strain 2 %,
Temperature 120 °C
 80.0 MPa
@Strain 1 %,
Temperature 60.0 °C
 80.0 MPa
@Strain 1.5 %,
Temperature 80.0 °C
 90.0 MPa
@Strain 4 %,
Temperature 150 °C
 95.0 MPa
@Strain 8.0 %,
Temperature 150 °C
 95.0 MPa
@Strain 2 %,
Temperature 80.0 °C
 100 MPa
@Strain 4 %,
Temperature 120 °C
 110 MPa
@Strain 6.0 %,
Temperature 120 °C
 120 MPa
@Strain 2 %,
Temperature 60.0 °C
 120 MPa
@Strain 1 %,
Temperature 0.000 °C
 120 MPa
@Strain 1 %,
Temperature -40.0 °C
 120 MPa
@Strain 1.5 %,
Temperature 23.0 °C
 125 MPa
@Strain 4 %,
Temperature 80.0 °C
 130 MPa
@Strain 6.0 %,
Temperature 80.0 °C
 150 MPa
@Strain 4 %,
Temperature 60.0 °C
 200 MPa
@Strain 2 %,
Temperature 0.000 °C
 200 MPa
@Strain 3 %,
Temperature 23.0 °C
 210 MPa
@Strain 2 %,
Temperature -40.0 °C
Elongation at Break 3.0 %ISO 527 Type 1A
Tensile Modulus 11400 MPaISO 527 Type 1A
Flexural Strength 290 MPaASTM D790
Flexural Modulus 9500 MPaISO 178
 9800 MPaASTM D790
Izod Impact, Unnotched 12.2 J/mASTM D256
Izod Impact, Notched (ISO) 13.0 kJ/m²ISO 180/1A
Charpy Impact Unnotched 95.0 kJ/m²ISO 179/1eU
Charpy Impact, Notched 13.5 kJ/m²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Surface Resistance 6.00e+14 ohmIEC 60093
Dielectric Constant 3.7IEC 60250
Dielectric Strength 34.0 kV/mmIEC 60243
Dissipation Factor 0.010IEC 60250
Comparative Tracking Index 600 VSol A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Transverse to Flow 22.0 µm/m-°C
@Temperature 23.0 - 85.0 °C
ISO 11359
Melting Point 263 °CISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 255 °CISO 75/Af
Flammability, UL94 HB
@Thickness 0.800 mm
ISO 1210
 HB
@Thickness 1.60 mm
ISO 1210
 HB
@Thickness 3.20 mm
ISO 1210
Oxygen Index 23 %ISO 4589
 
Processing PropertiesOriginal ValueComments
Processing Temperature 270 - 280 °CCompression zone
 280 - 290 °CMixing zone
Feed Temperature 265 - 275 °C
Mold Temperature 70.0 - 100 °C
Drying Temperature 80.0 °C
Moisture Content <= 0.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Domo TECHNYL® A 218 V35 Black 21 N PA 66 35% Glass Reinforced, Conditioned

PSOLVAY832 / 218560

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.