MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Huafon JF-P-5675/JF-I-5118 Polyester
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester TPE

Material Notes: Characteristics: Medium hardness

Applications: For man/woman shoes and casual shoes

Information provided by Zhejiang Haufon New Materials Corp., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.260 - 0.300 g/ccFree rise foam density
 0.550 - 0.600 g/ccMolded
 1.16 - 1.18 g/cc
@Temperature 40.0 °C
JF-P-5675
 1.18 - 1.20 g/cc
@Temperature 40.0 °C
JF-P-5118
Viscosity 200 - 500 cP
@Temperature 40.0 °C
JF-P-5118
 900 - 1400 cP
@Temperature 40.0 °C
JF-P-5675
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength >= 6.50 MPa
Elongation at Break >= 450 %
Tear Strength >= 25.0 kN/m
Abrasion >= 20[%] NBS abrasion resistance
 
Processing PropertiesOriginal ValueComments
Mold Temperature 45.0 - 55.0 °C
 
Descriptive Properties
AppearanceLiquid or waxy40°C, JF-P-5675
 Transparent and pure liquid40°C, JF-I-5118
Asker A Hardness57-62
Asker C Hardness70-75
Cream time7-9 sec
Demold time4-5 min
Flexing resistanceNo crack-10°C, Breakage length
Material Temperature38-42°C
P+C/l Mix ratio100/100-105
Rise time28-30 sec

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHUAF001 / 294944

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.