MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Ultramid® A 50H1 Black LBO 129 Nylon 66, Heat Stabilized, Flame Retardant, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Heat Stabilized; Nylon 66, Unreinforced, Flame Retardant

Material Notes: Product Description: Ultramid® A 50H1 Black LBO 129 is an unreinforced polyamide 66 based on a non-phosphorous and non-halogenated flame retardant system, heat stabilized, for injection molding. This flame retardant grade, offers excellent filling qualities combined with good stiffness. European Railways Certifications – EN 45545-2 HL2; European Railways Certifications – EN 45545-2 HL3

Availability: North America

Additive: Flame Retardant; Heat Stabilizer

Features: Flame Retardant; Good Moldability; Good Stiffness; Halogen Free; Heat Stabilized; Low (to None) Phosphorus Content

Agency Ratings: EC 1907/2006 (REACH); EN 45545; UL QMFZ2

RoSH Compliance: RoSH Compliant

Appearance: Black; Natural Color

Forms: Pellets

Processing Method: Injection Molding

Resin ID (ISO 1043): PA66 FR(30)

Information provided by BASF Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.16 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 7250 psiISO 527-2
Tensile Strength, Yield 7250 psiISO 527-2
Elongation at Break >= 100 %ISO 527-2
Tensile Modulus 547000 psiISO 527-1
Flexural Strength 7250 psiASTM D790
 7980 psiISO 178
Flexural Modulus 247000 psiISO 178
 254000 psiASTM D790
Charpy Impact Unnotched NBISO 179/1eU
Charpy Impact, Notched 3.30 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+12 ohm-cmIEC 62631-3-1
Surface Resistance 1.00e+14 ohmIEC 62631-3-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBASG2077 / 310770

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.