MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Celanese ZENITE ZE55801 LCP, 30% Specialty
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP); Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled

Material Notes: Zenite« ZE55801 is a 30% glass fiber reinforced and lubricated liquid crystal polymer for injection molding and It is specifically suitable for electroless plating.

Information provided by Celanese Corporation.

Key Words: 30% glass reinforced, lubricated, designed for enhanced electroless plating
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 140 MPa5mm/min; ISO 527-2/1A
Elongation at Break 4.0 %5mm/min; ISO 527-2/1A
Tensile Modulus 11099 MPa1mm/min; ISO 527-2/1A
Flexural Strength 175 MPaISO 178
Flexural Modulus 11130 MPaISO 178
Izod Impact, Notched (ISO) 50.5 kJ/m²ISO 180/1A
Izod Impact, Unnotched (ISO) 56.6 kJ/m²
@Temperature 23.0 °C
ISO 180/1U
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+13 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohmIEC 60093
Comparative Tracking Index 150 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 3.00 µm/m-°CISO 11359-2
CTE, linear, Transverse to Flow 69.0 µm/m-°CISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 260 °CISO 75-1, -2
Flammability, UL94 V-0
@Thickness 1.50 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 40.0 - 150 °Ccavity
Melt Temperature 330 - 350 °C
Drying Temperature >= 150 °C
Dry Time 3 hour
Moisture Content 0.010 %Necessary low maximum

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese VECTRA A435 LCP, 35% Specialty
Celanese VECTRA A430 LCP, 25% Specialty
Celanese ZENITE 6130L LCP, 30% Glass Reinforced
Celanese VECTRA A230 LCP, 30% Specialty
Celanese VECTRA B230 LCP, 30% Carbon Fiber

PHCS518 / 123933

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.