MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC XENOY™ X4820 PC+PBT (Americas)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced

Material Notes: XENOY X4820 is a high modulus PC/PBT Blend. This resin provides high chemical resistance, excellent impact, very low creep, low CTE, excellent fatigue and dimensional stability.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.25 g/ccASTM D792
Density 1.26 g/ccISO 1183
Water Absorption 0.42 %23°C/sat; ISO 62
Moisture Absorption 0.140 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0095 - 0.011 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 10 g/10 min
@Load 5.00 kg,
Temperature 250 °C
ASTM D1238
 12 g/10 min
@Load 5.00 kg,
Temperature 265 °C
cm³/10 min; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 52.0 MPa50 mm/min; ISO 527
 58.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 57.0 MPa50 mm/min; ASTM D638
 58.0 MPa50 mm/min; ISO 527
Elongation at Break 100 %50 mm/min; ISO 527
 140 %50 mm/min; ASTM D638
Elongation at Yield 4.2 %50 mm/min; ASTM D638
 4.2 %50 mm/min; ISO 527
Tensile Modulus 3000 MPa1mm/min; ISO 527
 3200 MPa50 mm/min; ASTM D638
Flexural Yield Strength 87.0 MPa2 mm/min; ISO 178
 91.0 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2850 MPa2 mm/min; ISO 178
 2900 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 700 J/mASTM D256
 150 J/m
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 55.0 kJ/m²80*10*4; ISO 180/1A
 15.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 60.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 60.0 JASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 75.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 75.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
CTE, linear, Transverse to Flow 110 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 110 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 94.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 98.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 130 °CRate B/50; ASTM D1525
 132 °CRate B/50; ISO 306
 134 °CRate B/120; ISO 306
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 250 - 265 °CInjection Molding
Zone 1 240 - 260 °C
Zone 2 245 - 265 °C
Zone 3 250 - 270 °C
Melt Temperature 255 - 275 °C
Mold Temperature 40.0 - 90.0 °C
Drying Temperature 110 °CInjection Molding
Dry Time 4.00 - 6.00 hourInjection Molding
 8.00 hourCumulative; Injection Molding
Moisture Content 0.020 %
Back Pressure 0.300 - 0.700 MPa
Shot Size 50 - 80 %
Vent Depth 0.00130 - 0.00200 cm
Screw Speed 40 - 80 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10848 / 244315

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.