MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Ravago Manufacturing Americas Hylac® HF96 ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.

Information provided by Ravago.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.03 g/ccASTM D792
Linear Mold Shrinkage 0.0030 - 0.0070 cm/cm0.125 in; ASTM D955
Melt Flow 3.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 8.5 g/10 min
@Load 3.80 kg,
Temperature 230 °C
Cond I; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 102ASTM D785
Tensile Strength, Yield 6200 psiASTM D638
Elongation at Break 30 %ASTM D638
Tensile Modulus 360000 psiASTM D638
Flexural Yield Strength 9200 psiASTM D790
Flexural Modulus 335000 psiASTM D790
Izod Impact, Notched 4.60 ft-lb/in0.25 in; ASTM D256
 5.50 ft-lb/in73°F, 0.125 in; ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmASTM D257
 
Thermal PropertiesOriginal ValueComments
CTE, linear 64.0 µin/in-°F
@Temperature -40.0 - 176 °C
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 203 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 188 °FUnannealed; ASTM D648
Vicat Softening Point 210 °FASTM D1525
Flammability, UL94 HB
@Thickness 1.50 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 355 - 390 °F
Middle Barrel Temperature 390 - 430 °F
Front Barrel Temperature 420 - 455 °F
Nozzle Temperature 410 - 445 °F
Melt Temperature 465 °F
Mold Temperature 120 - 140 °F
Moisture Content <= 0.10 %
Injection Pressure 850 - 1000 psi
Back Pressure 70.0 - 140 psi
Shot Size 40 - 80 %
Screw Speed 50 - 90 rpm
 
Descriptive Properties
Holding Pressure710 to 850 psi
Injection RateSlow-Moderate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Albis Plastics ABS 01A HI01 Unreinforced
INEOS Styrolution Terluran® EGP-7 ABS
INEOS Styrolution Terluran® HI-10 ABS
Aclo Accucomp ABS ABS846HL High Flow Medium Impact Grade
Ineos ABS Lustran® 648

PENTA031 / 36040

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.