MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Crosspolimeri FRAGOM G/471 Flame Retardant Halogen Free Polyolefine
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: FRAGOM: is the trade-mark of our flame retardant halogen free polyolefine compounds.

FRAGOM G/471: flame retardant cross-linkable compound having good temperature index and oxygen index, suitable for cable sheathing and insulation. It is a conveniently grafted compound able to react in presence of moisture and of a catalyst. We suggest our catalyst type MAC/400 PS to extrude with low compression screw. To use in solar cables sheathing ( TUV ) we suggest to add 8/10 % of catalyst MAC/400 PSUV REACTION BETWEEN GRAFTING AND CATALYST These two compounds, separately stored, must be mixed before starting extrusion in the ratio: GRAFTING/CATALYST 95/5

Certify: BS7211 EI5, VDE0207 HJ1, TUV2pfg1169-082007, EN 50618, IEC 60502 XLPE

Information provided by Crosspolimeri S.P.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.42 g/cc1.42 g/ccWith catalyst; ASTM D792
Melt Flow 4.0 - 8.0 g/10 min
@Load 21.6 kg,
Temperature 150 °C
4.0 - 8.0 g/10 min
@Load 47.6 lb,
Temperature 302 °F
ASTM D1238
Storage Temperature 12.0 °C53.6 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 3939ASTM D2240
Tensile Strength >= 12.5 MPa>= 1810 psiIEC 60811
 >= 14.0 MPa
@Temperature 135 °C,
Time 605000 sec
>= 2030 psi
@Temperature 275 °F,
Time 168 hour
Heat Ageing; IEC 60811
Elongation at Break 300 %300 %IEC 60811
 318 %
@Temperature 135 °C,
Time 605000 sec
318 %
@Temperature 275 °F,
Time 168 hour
Heat Ageing; IEC 60811
 
Thermal PropertiesMetricEnglishComments
Oxygen Index 34 %34 %ASTM D2863
 
Processing PropertiesMetricEnglishComments
Zone 1 80.0 - 90.0 °C176 - 194 °F
Zone 2 100 - 115 °C212 - 239 °F
Zone 3 145 °C293 °F
Zone 4 160 °C320 °F
Die Temperature 170 °C338 °F
Head Temperature 165 °C329 °F
 
Descriptive Properties
Corrosivity of gases evolved>4,4 pHIEC 60754-2
Halogen Content< 0,3%IEC 60754-1
Hot Set Test<100%250°C - 20 N/cm2, IEC 60811
 0Residual Value, IEC 60811

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCROS062 / 294146

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.