MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Versalis Extir® EH 2000 Expandable Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Expanded Polystyrene (EPS)

Material Notes: Extir EH 2000 is an expandable polystyrene in the form of spherical beads of fine particle size, with a low pentane content as blowing agent. Extir does not contain CFC or HCFC. Extir EH 2000 is used for very fast cycle production of shape mouldings with thin sections and medium to very high density. This grade is also characterised by very short maturing time, even at very high density, excellent processability, good fusion, good surface finishing and very good dimensional stability.

Applications: Extir EH 2000 is a very fast cycling grade used for production of moulded items with thin sections (usually less than 8 mm) and also of skin moulded articles. Finished products exhibit high fusion, high resistance to impact / mechanical stress, and an outstanding dimensional stability. Extir EH 2000 is suitable for the production of food packaging and for food contact applications. Typical applications are: • industrial and protection packaging • food trays, ice cream containers, frozen dessert packaging • high precision mouldings • insulating soles for ski boots • containers and loaders for automated manufacturing in the electronics sector • reusable seed trays

It is recommended to keep the product in a dry well ventilated store between 15-20°C. For product packaged in octabins the guaranteed shelf-life is one month; product in steel drums has a six months guaranteed shelf-life. During the processing of Expandable Polystyrene any sparkle or flame must be avoided and smoking should be forbidden. An adequate electrical grounding of machinery and of pneumatic transport lines is recommended. For further information concerning storage, packaging and processing precautions please refer to "Styrenics - Technical data sheets" and to the "Extir Safety Data Sheet". This grade complies by composition with the requirements set by the main regulations for plastics intended for food contact (including the EEC directive 90/128).

Processing: Extir EH 2000 can be easily pre-expanded on conventional equipment over a wide density range (from 21 to 80 kg/m³) despite its low pentane content. This product needs minimum maturation times (from 1 to 48 hours), even at high density. Moreover the steaming cycle is nearly not influenced by the maturation time. Due to excellent processability and low pentane content, it is possible to operate with very fast cycle times (mainly by reducing the cooling times) and with low steam pressures. Moulded items exhibit a very high fusion level, excellent surface finishing, good mechanical properties and an excellent dimensional stability. Extir EH 2000 can be moulded on all types of shape moulding machines.

Information provided by Polimeri Europa

Versalis is the Eni subsidiary containing the plastics and rubber businesses.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.590 - 0.630 g/cc
Density 0.0220 - 0.0800 g/cc
Apparent Bulk Density 0.0210 g/ccOn a discontinuous pre-expander
 0.0250 g/ccOn a continuous pre-expander after one expansion
Particle Size 400 - 750 µm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NOVA Chemicals Arcel 730 70% PS/30% PE Interpolymer
Jackon JACKOCELL® R311 Expanded Polystyrene Packaging and Shape Molding
BorsodChem ONGROSTYR F-I Expandable Polystyrene (EPS)
NOVA Chemicals Expandable Polystyrene (EPS) 33MB Expandable Polystyrene Resin
Premix Thermoplastics PRESEAL 5020 Ni-Coated Graphite

PENH84 / 35798

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.