MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials GBL-900  (discontinued **)
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: VTR-8650 is a 68% fluorine peroxide cured polymer similar to Viton® GBL-900 but with significantly improved processing and curing characteristics. VTR-8650 utilizes Advanced Polymer Architecture technology which includes a new peroxide cure site along with an optimized molecular weight distribution designed to deliver a polymer which:
  • Cures exceptionally fast to a high state of cure
  • Shows improved mold release/mold fouling properties compared to Viton® GBL-900 and 200
  • Shows improved mold flow, less shear sensitivity, and lower extruder die swell for a ~65 Mooney FKM
  • Shows excellent physical properties with high elongation, both original and aged
  • Shows similar heat, fluids, and low temperature resistance compared to Viton® GBL-900 and 200
  • Shows improved water resistance/volume swell in water compared to Viton® GBL-900 and 200
  • Shows excellent compression set resistance with either low or no postcure

It is recommended if mixing in an internal mixer to use at least a 70% load factor. The recommended process aid for VTR-8650 is 0.5 phr of Armeen® 18D.

Information provided by manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Mooney Viscosity 86
@Temperature 121 °C
ML-10 (gum)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 73Cured 7 min at 177°C and Post Cured 16 hr at 232°C
Tensile Strength, Ultimate 20.9 MPaCured 7 min at 177°C and Post Cured 16 hr at 232°C
Tensile Strength, Yield 0.000750 GPa10% Modulus, Cured 7 min at 177°C and Post Cured 16 hr at 232°C
Elongation at Break 174 %Cured 7 min at 177°C and Post Cured 16 hr at 232°C
100% Modulus 0.00730 GPa
@Strain 100 %
Cured 7 min at 177°C and Post Cured 16 hr at 232°C
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg -15.8 °CDSC, modulated, midpoint
 
Component Elements PropertiesOriginal ValueComments
Fluorine, F 68 %
 
Descriptive Properties
Formulation as Tested100Viton® GBL-900
 3Zinc Oxide
 3Diak™ 7 (TAIC)
 3Luperox® 101-XL peroxide
 30N990 Carbon Black

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CHT Group MM810 Low Tear Condensation Cure 2-Part Molding Rubber
Chemours Viton® GBL-900 Fluoroelastomer (FKM)
Overview of materials for PVC, High Impact
Omnova Solutions Sunigum® P95 Acrylate Elastomer
Dynasol Solprene® 200P Polybutadiene Rubber

PDVDA57 / 34026

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.