MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Avient Dynalloy™ OBC8000-T40 Thermoplastic Elastomer (TPE)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Dynalloy™ OBC8000-T40 is an easy processing, general processing TPE utilizing the unique rubber properties of Dow INFUSE™ Olefin Block Copolymers. Designed for a wide variety of applications, including applications requiring FDA compliances - Adhesion to Polypropylene - Enhanced Flow - Excellent Colorability - Warm, Non-tacky, Rubbery

Color concentrates with polypropylene (PP), ethylene vinyl acetate (EVA), or low density polyethylene (LDPE) carriers are most suitable for coloring Dynalloy™ OBC8000-T40. Improved color dispersion can be achieved by using higher melt flow concentrates (with a melt flow from 25 - 40 g/10 min). Typical loadings for color concentrates are 1% to 5% by weight. Liquid color can be used, but mineral oil based carriers may have a significant effect on the final hardness value. Concentrates based on PVC should not be used. A high color match consistency can be obtained by using precolored compounds available from GLS. The final determination of color concentrate suitability should be determined by customer trials. Purge thoroughly before and after use of this product with a low flow (0.5 - 2.5 MFR) polystyrene (PS) or polypropylene (PP). Regrind levels up to 20% can be used with Dynalloy™ OBC8000-T40 with minimal property loss, provided that the regrind is free of contamination. To minimize losses during molding, the melt tempetature should remain as low as possible. The final determination of regrind effectiveness should be determined by the customer. Dynalloy™ OBC8000-T40 has good melt stability. Maximum residence times may vary, depending on the size of the barrel. Generally, the barrel should be emptied if it is idle for periods of 8 - 10 minutes or longer. Drying is not Required Injection Speed: 1 to 3 in/sec 1st Stage - Boost Pressure: 200 to 900 psi 2nd Stage - Hold Pressure: 20% of Boost Hold Time (Thick Part): 4 to 10 sec Hold Time (Thin Part): 1 to 4 sec

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.878 g/ccASTM D792
Viscosity 8300 cP
@Shear Rate 11200 1/s,
Temperature 200 °C
ASTM D3835
 37000 cP
@Shear Rate 1340 1/s,
Temperature 200 °C
ASTM D3835
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 4310 sec; ASTM D2240
Tensile Strength at Break 3.10 MPa
@Temperature 23.0 °C
Die C2 hr; ASTM D412
Tensile Stress at Strain 1.05 MPa
@Strain 100 %,
Temperature 23.0 °C
Die C2 hr; ASTM D412
 1.57 MPa
@Strain 300 %,
Temperature 23.0 °C
Die C2 hr; ASTM D412
Elongation at Break 790 %
@Temperature 23.0 °C
Die C2 hr; ASTM D412
Compression Set 24 %
@Temperature 23.0 °C,
Time 79200 sec
ASTM D395B
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 166 - 188 °C
Middle Barrel Temperature 177 - 199 °C
Front Barrel Temperature 199 - 221 °C
Nozzle Temperature 199 - 221 °C
Melt Temperature 193 - 227 °C
Mold Temperature 26.7 - 37.8 °C
Back Pressure 0.000 - 0.552 MPa
Screw Speed 50 - 100 rpm
 
Compliance PropertiesOriginal ValueComments
FDA YesUnspecified Rating
 
Descriptive Properties
AppearanceTranslucent
FeaturesGood Colorability
 Good Flow
FormsPellets
Generic MaterialTPE
Generic NameThermoplastic Elastomer (TPE)
Processing MethodExtrusion
 Injection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
RoHS ComplianceRoHS Compliant
Suggested Max Regrind20%
UsesConsumer Applications
 Overmolding
 Soft Touch Applications
 Transparent or Translucent Parts

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Makrolon® LED2245 Polycarbonate
Celanese Celstran® PP-GF30-02 PP, 30% Glass Reinforced
Envalior Arnitel® EL550 TPC-ET, Injection Molding
Envalior Arnitel® EB463 TPC-ET, Blow Molding Grade
Avient OnFlex™ S EH 40A-3S7001 Thermoplastic Elastomer (TPE)

PH0POL1169 / 145738

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.