MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
NAECO® ELKONIUM® 405 palladium based alloy
Categories: Metal; Nonferrous Metal; Precious Metal; Palladium Alloy

Material Notes: Palladium belongs to the platinum group of metals and like platinum is highly resistant to atmospheric corrosion; however, it begins to tarnish at temperatures above 400°C. It has a high melting point (1552(C) and, like platinum, resists arc formation. Its low electrical conductivity (16% IACS) limits its application to low current circuits. It costs much less than platinum, and is used as a lower cost alternative. Economics normally dictate that it be supplied as a composite contact with a thin contact metal facing silver brazed to a nickel-plated steel rivet, screw, or projection weld button backing.

ELKONIUM® 405 is a palladium base alloy sold by CMW containing sufficient ruthenium to increase the hardness. Its corrosion resistance is similar to that of palladium and its resistance to transfer is greater than that of pure palladium. It is used in thermostats and other sensitive low voltage devices, and is a lower cost alternative to platinum alloys for these applications.

Information provided by NAECO, LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 12.0 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell 15T 85annealed
 92cold worked
Tensile Strength, Ultimate 70000 psiannealed
 100000 psicold worked
Elongation at Break 2.0 %cold worked
 13 %annealed
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000287 ohm-cm6 % IACS
 
Component Elements PropertiesOriginal ValueComments
Palladium, Pd 89 %
Ruthenium, Ru 11 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Palladium Alloy
Overview of materials for Refractory Metal
NAECO® ELKONIUM® 301 platinum based alloy
MarkeTech 97-2-1 Tungsten Alloy, AMS-T-21014 Class 4
Johnson Matthey Palladium w/ 5% Ruthenium+Gallium Jewelry Alloy

NCMV910 / 192388

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.