MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
HB Fuller Hydra FAST-EN ™ DC-13634 Adhesive
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: Product Description: Hydra FAST-EN ® DC-13634 spray system is a two part spray-able adhesive designed to bond open cell urethane foams. It can also be used to bond open cell urethane foams to other porous or non-porous surfaces including other open or closed cell foams, some woods and metals, and various plastics and fabrics. The adhesive has good wet grab and can produce immediate bonds. The system is solventless, user-friendly and addresses many of the common problems encountered with other two part systems. Other applications where the use of solvent based, flammable and non-flammable systems are a concern for either health or environmental reasons may also be suitable candidates for the use of this product. Product Features:
  • Water-based -- Non toxic, easy clean up
  • Two-part -- Ratio not critical to end performance
  • Fast tack -- Parts can be mated immediately after spraying
  • Delayed mating -- If desired, parts can be mated as long as 10 minutes after spraying
  • Color tinted -- Aids in noting coverage and uni-formity: Standard color is charcoal. Other colors are available.
  • Environmentally Friendly -- Neither wet nor dry adhesive is considered a RCRA hazardous waste
  • Equipment friendly -- 2 parts are mixed external to the spray gun
  • Shear stability -- Part A and Part B are not affected by normal shear forces generated by mechanical pumps or mixers
  • Temperature range -- The mixed adhesive when dry has a use range of -50 to 190°F
  • Shelf life -- When stored between 40°F and 80°F in unopened containers: Part A : 4 months, Part B: 12 months

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/ccPart A
 1.115 g/ccPart B
Solids Content 15 %Part B
 47.5 %Part A
pH 3.5Part B
 12Part A
Viscosity 500 cP#2 @ 10 rpm
 
Processing PropertiesOriginal ValueComments
Shelf Life 4.00 MonthPart A
 12.0 MonthPart B
 
Descriptive Properties
Base compoundPolychloroprenePart A
 Zinc SulfatePart B
ColorBlack (dried)Part A
 Charcoal (wet)Part A
 ClearPart B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHBFULL121 / 316912

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.