MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Nitriflex Nitrigum 25 FK Styrene Butadiene Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Food grade polymer. Fully compatible with resins and paraffins, normally used in gum bases. Presents a soft mastication, ideal for chewing gums. When presented in granules, allows shorten mixing time and better homogenization. Available in the versions Kosher (FK), with BHA (FA) and granulated (G).

Applications:

Information provided by Dax Resinas

FDA-21-CRF172.615 E FCC-V

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles 0.00 - 1.0 %Method B-003; ASTM D5668
Mooney Viscosity 46 - 58
@Temperature 100 °C
MML1+4, Method B-002; ASTM D1646
Ash 0.00 - 0.50 %ASTM D5667
 
Chemical PropertiesOriginal ValueComments
Styrene Content 0.00 - 0.020 %Residual Styrene; FCC
 22 - 26 %ASTM D5775
 
Descriptive Properties
AppearanceWhite to yellowish
BHT (%)0-0.4CAF-MET-615

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Precision Polymer Engineering N65E Nitrile Rubber
Precision Polymer Engineering N50M Nitrile Rubber
Nitrile Rubber (NBR, Acrylonitrile-Butadiene Rubber)
Nitriflex SB-1009 Styrene Butadiene Copolymer
Nitriflex SB-1009 G Styrene Butadiene Copolymer

PDAX060 / 29485

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.