MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
KEP Kepital® FV-30A Acetal Copolymer, Anti-static
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes:

Information provided by KEP Americas.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Linear Mold Shrinkage, Flow 0.020 cm/cmt = 3 mm
Melt Flow 29 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 63.0 MPa50 mm/min; ISO 527
Elongation at Break 25 %50 mm/min; ISO 527
Elongation at Yield 8.0 %50 mm/min; ISO 527
Flexural Strength 88.0 MPaISO 178
Flexural Modulus 2580 MPaISO 178
Charpy Impact, Notched 5.00 kJ/m²ISO 179
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 1.00e+15 ohmIEC 60093
Dielectric Strength 19.0 kV/mmIEC 60243
 
Thermal PropertiesOriginal ValueComments
Melting Point 165 °CISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 97.0 °CISO 75

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company RTP 1899 X 136863 J Acrylic (PMMA); ESD Protection - Permanently Static Dissipative - Transparent
Premix Thermoplastics PRE-ELEC® ESD 7140 Static Dissipative Thermoplastic Compound
Premix Thermoplastics PRE-ELEC® ESD 5510 Static Dissipative Thermoplastic Compound
Premix Thermoplastics PRE-ELEC® ESD 4400 Static Dissipative Thermoplastic Compound
Kolon KOCETAL® VT702 Anti-Static Grade Acetal Resin

PKEP9907 / 185583

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.