MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Momentive Performance Materials Silopren LSR 47X9 Liquid Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: The Silopren LSR 47X9 series is a two-component self-bonding liquid silicone rubber for injection molding processes. Silopren LSR 47X9 offers primerless adhesion to a variety of substrates including polycarbonate, polybutylene terephthalate (PBT), and co-polyesters. The Silopren LSR 47X9 series offers primerless adhesion to a variety of thermoplastic substrates, which can allow greater cost efficiency in the manufacture of high-volume multi-component injection molded or insert molded parts. The self-bonding nature of the Silopren LSR 47X9 series allows adequate bond strength to be reached without the need for pretreatment of the substrates surface. Like standard liquid silicone rubbers, Silopren LSR 47X9 also has high temperature stability, and can easily be pigmented with LSR color pastes. Key Features and Typical Benefits of Silopren LSR 47X9: Primerless adhesion to polycarbonate, PBT, and co-polyesters, No adhesion to the mold, High thermal stability. Potential Applications: Membranes and diaphragms. Surgical and dental instrument grips. Other hard-soft combinations.

Information provided by Momentive Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMOMEN9964 / 265779

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.