Hostacom PPU X9067HS 104908 is an unfilled PP copolymer, with high melt flow rate, high toughness and increased stiffness. This grade is delivered in 104908 color version. This product is also available in other colors, new colors can be developed depending on customer requirements. Applications : Automotive Parts, Interior Trims.Information provided by LyondellBasell. |