MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Huntsman AVALON® 98 AB Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Introduction: AVALON 98 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 98 AB is part of the AVALON Performance Range and offers a premium soling material for sports footwear and top-pieces. The features offered include:
  • Durability
  • Excellent surface definition
  • Abrasion resistance
  • Flex resistance
  • Phthalate free TPU

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.23 g/ccISO 2781
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 98ISO 868
Hardness, Shore D 56ISO 868
Tensile Strength at Break 40.0 MPaISO 37
Elongation at Break 400 %ISO 37
100% Modulus 0.0170 GPa
@Strain 100 %
ISO 37
300% Modulus 0.0290 GPa
@Strain 300 %
ISO 37
Flexural Modulus 135 MPaISO 178
Tear Strength 165 kN/mISO 34B
Abrasion 35mm3; ISO 4649
Compression Set 20 %ISO 815
 
Processing PropertiesOriginal ValueComments
Feed Temperature 25.0 - 35.0 °C
Rear Barrel Temperature 200 - 210 °C
Middle Barrel Temperature 205 - 215 °C
Front Barrel Temperature 210 - 220 °C
Nozzle Temperature 200 - 210 °C
Mold Temperature 25.0 - 50.0 °C
Injection Pressure 2.00 - 10.0 MPa
Hold Pressure 1.00 - 5.00 MPa
Back Pressure 0.0300 - 0.300 MPa
Screw Speed 20 - 80 rpm
 
Descriptive Properties
Compression Ratio2-3:1
L/D Ratio20-25:1
Ross Flex-10°C, BS 5131
Typical Screw Diameter40-120 nm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Bamberger Polymers Bapolene® EVA-1120 Ethylene Vinyl Acetate (EVA)
Huntsman AVALON® 60 DB Thermoplastic Polyurethane
Elkem Silicon Injection Grade
Braskem VA2019A EVA Foam Copolymer
Bamberger Polymers Bapolene® EVA-1122 Ethylene Vinyl Acetate (EVA)

PHUQ165 / 159538

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.