MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Extreme Materials from MCAM
Visit Mitsubishi Chemical Advanced Materials for Extreme Materials - high performance plastic machining stock engineered to replace metals such as nickel alloys or stainless steel.

(Viewing data as-entered. Click here to return)
P & P Technology BS3075 NA13 Monel Wire
Categories: Metal; Nonferrous Metal; Nickel Alloy

Material Notes: Alloy 400L

Wire Diameter 0.11mm

Information provided by P & P Technology

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Electrical PropertiesOriginal ValueComments
Shielding Effectiveness 38 dB
@Frequency 10000 Hz
H-Field, Magnetic
 40.5 dB
@Frequency 100000 Hz
H-Field, Magnetic
 45.5 dB
@Frequency 1e+6 Hz
H-Field, Magnetic
 62.5 dB
@Frequency 1e+10 Hz
P-Field, Electrical
 81 dB
@Frequency 1e+9 Hz
P-Field, Electrical
 98.5 dB
@Frequency 4.00e+8 Hz
P-Field, Electrical
 106 dB
@Frequency 1.10e+8 Hz
P-Field, Electrical
 107 dB
@Frequency 1e+7 Hz
E-Field, Electrical
 124.5 dB
@Frequency 1e+6 Hz
E-Field, Electrical

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Special Metals MONEL® Alloy K-500
P & P Technology Monel-BS3075 (NA13) Knitted Cored Shielding Mesh
Special Metals MONEL® Alloy 400
Special Metals MONEL® Alloy 450
MetalTek MTEK B Cast UNS N24030 Nickel-Copper Alloy

PPPTEC017 / 133481

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.